page_banner

Products

750ml Swing Top Bottles Wholesale

Short Description:

If you’re selling a retro brand of drink, look no further than our 1000ml Glass Swing Top Bottle. It is the largest swing top bottle in our collection, with a large  litre capacity. It boasts a vintage shape, with faceted sides that offer good grip and just look fantastic! 


Product Detail

Product Tags

If you're selling a retro brand of drink, look no further than our 1000ml Glass Swing Top Bottle. It is the largest swing top bottle in our collection, with a large litre capacity. It boasts a vintage shape, with faceted sides that offer good grip and just look fantastic! Best of all, this bottle comes fitted with a ceramic stopper cap, which is locked into place with a pull down metal clasp.

In our opinion, 1000 ml glass shaper is very suitable for filling all kinds of wine, juice, sauce, edible oil, etc.You can even bottle up your specialist spirits and wines with this unique bottle and separate your brand from your competitors.

Causes and solutions of glass bottle shoulder defects

1. Shoulder crack. Surface crack on shoulder. Droplet temperature too high or too low. The opening of the initial die or forming die is not smooth. Overblown air pressure. Improper fit of forming die and die bottom. Forming die clamp wear seriously. Mold temperature is too high.
2. Thin shoulders. Bottle shoulder is partially or wholly thin. The droplet temperature is high or uneven. Droplet shape too long or too short. The material is not straight. The initial mold is too hot. Too much oil on the initial mould. The positive blow starts too late.Inverted blowing pressure is small or time is short
3. Bottle shoulder is insufficient (flat shoulder, concave bang). The bottle shoulder is not fully formed. Droplet temperature too high or too low. The droplet shape is not good or the thin material is not right, and the friction on the material path is large. Improper position of positive blow head or too small positive blow pressure. Positive blow time too short.Backblowing pressure is too high or time is too long, initial shape is too hard.Insufficient reheating time. Too cold for primary or forming dies.
At present, the market with strong demand for glass bottles generally exists, and the food industry and beverage manufacturing industry are the most important market for daily glass packaging products.